Ansco 135

Water @ 125F
Elon
Sod. Sulfite
Hydroquinone
Sod. Carbonate
Pot. Bromide
Water to make
750ml
1.6g
24g
6.6g
24g
2.8g
1.0L

For use, dilute 1 part stock solution with 1 part water. A properly exposed print will be fully developed at 68 deg F (20 deg C) in about 1 to 2 minutes. Complete development may be expected to take slightly longer with rough-surfaced papers than with semi-glossy or luster-surfaced papers. For greater softness, dilute the bath with water up to equal quantities of developer and water. To increase the warmth, add bromide up to double the amount in the formula. The quantity of bromide specified in the formula, however, assures rich, warm, well-balanced tones.